Page 121 - CITS - Welder - Trade Theory
P. 121

WELDER - CITS


                                                            ..
           Electrodes  affected  by  moisture  may  be  baked  before  use  by  putting  them  in  a  controlled  drying  oven  for
           approximately one hour at a temperature around 110 - 150°C. This should not be done without reference to the
           conditions laid down by the manufacturer. It is important that hydrogen controlled electrodes are stored in dry,
           heated conditions at all times.
           Warning:  Special  drying  procedures  apply  to  hydrogen  controlled  electrodes.  Follow  the  manufacturer’s
           instructions.
           Remember a moisture-affected electrode:

           a  has rusty stub end.
           b  has white powder appearance in coating.
           c  produces porous weld.
           Always pick up the right electrode that will provide:

           a  good arc stability
           b  smooth weld bead
           c  fast deposition
           d  minimum spatters
           e  maximum weld strength

           f  easy slag removal.






















































                                                           108