           Direction of welding

           Move the blow pipe in a leftward direction along as straight line to complete the weld. (Fig 4)

             Fig 4



















              Maintain a constant 2-3mm of distance between the white cone of the flame and the sheet surface
              for a proper HEAT INPUT and avoidance of BACKFIRE.
           Inspection of weld

           Inspect the weld bead after cleaning properly with a wire brush, for a uniform width and height of the bead, uniform
           ripples, and proper depth of fusion. (Fig 5)


              Fig 5


















































                                                           197

                                           CITS : C G & M - Fitter - Exercise 54