WELDER - CITS





           Deposit the final covering run with and 120 - 140 amp current.
           Give side-to-side movement to the electrode not more than 2.5 times its dia.
           Use the same electrode angle as was used for the root bead.

              Note: Prevent the upper edge of the plate from melting off by not allowing the arc to concentrate
              more on the upper edge.
           Remove the slag with a chipping hammer.
           Clean the weld with a steel wire brush.

           Inspect the butt fillet weld and ensure:
           •  It has equal leg length with slight convexity
           •  The upper edge of the plate has not melted off
           •  it is free from surface defects.