           Weld similarly the 2nd run by using 5mmø filler rod dipped in flux with a soft oxidizing flame and get 1.5mm
           reinforcement and good bead up to the end of the joint. Fig 3.

                    Fig 3




















           Clean the bead and remove the flux residue on both sides of the joint.

           Inspect the joint for weld defects like porosity, incomplete penetration etc.